Woven tape uses polypropylene FDY filament. How can one choose the right filament to avoid breakage and fraying during production? 


Raw Materials and Filament Selection


To reduce breakage and fraying during the production process of woven tape, the quality of the polypropylene FDY filament itself must be controlled first. Preferentially select filament materials with fully formed spinning and shaping, uniform internal structure, low residual stress, and less tendency to fray or break under weaving stress. Pay attention to the appearance of the single filament to avoid purchasing products with inherent frayed fibers, nodes, or scratches. Such defects will continuously expand during high-speed weaving, resulting in batch fraying. Pay attention to the oiling state of the filament bundle, with uniform and moderate oil adhesion. Insufficient oiling causes excessive friction and obvious static electricity, leading to fraying; excessive oiling can cause the filament bundle to slip and shift, also affecting the stability of weaving. At the same time, confirm that the raw material formula is stable, reducing impurities and gel particles, and reducing the probability of the guide wire components wearing out the filament bundle. 


Selecting Filament Based on Weaving Conditions


Based on the type of loom, weaving speed, and weaving structure of the tape, select the filament. For fine and thin woven tapes, preferentially choose specifications with uniform filament and good cohesion; for thick and heavy-duty woven tapes, focus on categories with tighter filament structure and better anti-friction performance. The twist ratio of the filament is very crucial. The appropriate twist ratio can enhance the cohesion of the single filament and reduce the mutual sliding and frictional fraying during weaving. Too low twist ratio causes the filament bundle to be loose and prone to breakage and fraying; too high twist ratio causes the filament material to have high internal stress, and is more likely to break under stress. Also, pay attention to batch stability. The fluctuation of filament quality between different batches will cause the adjusted weaving process to no longer be suitable and intermittent breakage problems to occur. When purchasing, prefer suppliers with stable process control. 


Summary of Selection


Breakage and fraying are not only a problem of the filament material alone, but also related to guide wheels, yarn threading paths, and tension control. When selecting filament, use filament appearance, internal shaping, oiling state, and batch consistency as the core judgment points, and combine it with your own loom speed and matching specifications for the woven tape structure. After receiving the sample, it is recommended to conduct a small trial on the machine, observe the running state for a long time, confirm that the frayed fibers and breakage are stable, and then conduct batch purchases. If you need sample consultation, please feel free to contact us.